The issue of thin dry cement skin caused by the laitance of concrete.

Thin, brittle residue on the surface of new concrete and the thin layer formed after curing, which causes paint film to peel due to poor adhesion.

Causes include

  • The level of the laitance layer increases due to:
  • Too much water in the concrete mix (causing excessive laitance separation)
  • Excessive use of a trowel, resulting in a soft, weak surface film
  • Newly poured concrete being exposed to rain and poor curing conditions
  •  

Solutions

  • Determine the thickness of the laitance layer by leveling at the metal edge during the pouring of the new concrete surface
  • Choose an appropriate removal method such as acid etching, sandblasting, or shot blasting, grinding, polishing, or mechanical stripping
  • Apply a primer for adhesion with Beger Concrete Sealer. 1-2 coats, allowing to dry completely for 6-8 hours
  • Topcoat with Durathane / DuraGuard paint or acrylic paint such as BegerCool UV Shield / BegerCool Diamond Shield Plus